Kraft Heinz Eyes Super-spatial Atomic Layer Deposition Barrier
Kraft Heinz crowned Kalpana Systems—a Dutch technologist behind a ‘thin film with the precision of a single atom’—as the winner of Rethinking Materials’ recent Global Innovation Challenge. The emerging tech delivers advanced oxygen and moisture barriers to otherwise recyclable paper or mono-PE, without impacting recyclability.